GORE® TENARA®Sewing ThreadPROCESSING GUIDELINESFor seams thatoutlast the fabric.Successful sewing starts here GORE® TENARA® Sewing Thread is guaranteed to last for the life of the fabric in which it is sewn, making it the ideal sewing thread for outdoor and marine applications.GORE® TENARA® Sewing Thread can be sewn at 2,600 stitches per minuteor more. Because GORE® TENARA® Sewing Thread is made from expanded polytetrafluoro e thylene (ePTFE), the sewing process is slightly different from that used with typical polyester thread.Selecting and Balancing Your StitchYou can use GORE® TENARA® Sewing Thread with either a lockstitch or chainstitch type of sewing stitch. For either stitch, you should ensure the stitch is balanced to maximize seam strength and seam elasticity.Tension settings are crucial for balanced stitching. To set your lockstitch tension for GORE® TENARA® Sewing Thread:1. The starting bobbin tension setting should allow the bobbin to mimic a child’s yo-yo. The bobbin should slowly fall to the floor when suspended by the sewing thread.2. The bobbin thread tension should be adjusted as low as possible for a flat or running stitch on the bobbin thread. (See Figure 3).3. Gradually increase the tension on your top thread to obtain a balanced stitch and a tight seam.Note: To determine the stitch balance between the top and bottom threadsof a lockstitch, cut out a 10 cm length of your seam and pull out the top and bottom threads. Measure the length of both threads. If they are the same length, the stitch balance is adjusted properly.In a balanced lockstitch (stitch type 301), the topand bottom threads should meet in the middle of thefabric, forming distinct stitches on the top side andunderside o f the fabric as shown in Figures 1 and 2.If the top thread tension is too high or the bobbinthread tension too low, flat or running stitchesappear on the top of the fabric as shown in Figure 3.If the top thread tension is too low or the bobbinthread tension too high, flat or running stitchesappear on the underside of the fabric as shownin figure 4. The loose thread loops in Figure 4 arecommon when first using our heavier threads.A balanced chainstitch (stitch type 401) top threadappears similar to a balanced lockstitch as shown inFigure 5.The chainstitch top thread should be pulledcompletely to the underside o f the fabric, with thebottom thread appearing as shown in Figures 6 and 7.A poorly tensioned loose chainstitch bottom thread appears as in Figure 8.Figure 8Figure 3Figure 5Figure 7Figure 6Figure 2Figure 1Figure 4TroubleshootingWhen first using GORE® TENARA® Sewing Thread, you might find it helpful to use the following table as a guide to ensure the best performance of the thread. Once you are familiar with the characteristics of GORE® TENARA® Sewing Thread, your seams will last for the lifetime of the fabric.Possible Cause ActionExcess speed Reduce speedExcess thread tension Balance seam tension as described in“Selecting and Balancing Your Stitch.”Improper thread path Verify the thread path with your machinemanufacturer; use all recommended threadguides.Needle burr – bent or deflected needle strikes feed dog or throat plate Check the needle for burrs, and replace the needle if necessary.Burr on thread guide Use a magnifying glass to check all threadguides, and repair or replace any guides asneeded.Thread kinks Place spool socks over each spool of thread,extend spool sock up to first thread guide,or use thread brake on each spool.Broken thread take-up spring Replace.Bobbin and mechanical opener/bobbin case lifter not correctly adjusted Consult machine manufacturer or service technician.Type of Uneven Stitch ActionFlat or running top-stitch Decrease the tension of the top thread. Flat or running bottom-stitch Increase the tension of the top thread.Loops on the underside of the fabric (more common with heavy threads)Increase the tension of the top thread to approximately twice the tension used for TR/KTR thread, and balance the stitch as described in “Selecting and Balancing Your Stitch.”Possible Cause ActionImproper thread path Verify the thread path with your machinemanufacturer; use all recommended threadguides.Misaligned needle(Needle eye or cove should face the bobbin hook.)Rotate the needle clockwise until its eye faces the bobbin hook or is slightly rotated towards the hook as the hook approaches needle.Bent or deflected needle (Heavy fabrics can bend needle.)Replace the needle; if needles bend frequently, use a larger needle, or request stronger needles from your manufacturer.Incorrect needle size and/or needle construction(The needle may be too large, preventing the thread from consistently forming a loop. Special needles are available to reduce skipped stitches.)Use recommended needle size in the table, or try one size smaller. Contact needle supplier for skipped stitch reducing needles.Excess thread through the needle When pausing the machine, maintainpressure on the material with the presserfoot.Thread kinks Place spool socks over each spool of thread,or use thread brake on each spool.Worn bobbin hook(The hook should be pointed and sharp.)Replace the bobbin hook.Incorrect machine timing(The bobbin hook and needle must meet as per manufacturer specifications.)Use a timing gauge (available from your machine supplier) to adjust the machine timing per the manufacturer’s instructions.Incorrect bobbin hook placement: incorrect distance from needle Reposition the hook per the manufacturer’s instructions.Worn machine components(Needle bar, bearings, hook races, thread take-up spring, etc.)Replace components as needed. Reduce future wear by cleaning and lubricating per manufacturer’s recommendations.Chainstitching: incorrect looper position Reposition the looper closer to the needleper manufacturer’s instructions. If problemcontinues, consider replacing the looper. Chainstitching: Dull looper Replace looper, and ensure proper clearancefrom needle.Maintaining QualityMost importantly, please follow your sewing machine manufacturer’s maintenance schedule. Sewing machines are precision equipment that operates at high speeds. Cleaning and lubricating must be regularly scheduled to ensure continuous,trouble-free service. Oftentimes, problems with thread breaks and skipped stitches are due directly to misaligned and/or worn machine components. Many times these components wear out prematurely if they are not sufficiently cleaned and lubricated.You can ensure the best performance from GORE ® TENARA ® Sewing Thread by periodically checking the following parts and settings of the sewing machine:Part or Setting Visual Check ProblemSpool and thread stand alignment Spool center should be aligned with first thread guide and spool should beuprightMisalignment causes tension peaks and uneven stitches.Spool and threadstand distance Spool top should be within 6”–12”(15–30 cm) below of first thread guide Spool too close, spool will not unwind properly. Too far, thread “balloon” can catch on thread stand or other thread(double needle machines).Possible CauseAction Bobbin continues to rotate after themachine stops Use lightweight (aluminum) bobbins, anti-overrun washers, or “star washers” availablefrom your sewing machine manufacturer.When sewing double needle lockstitch applications, use an R needle pointshape on both left and right sides. If you experience skipped stitches or thread separation on the left needle, try using a CR type needle.Part or Setting Visual Check ProblemNeedle Point Point is sharp, and needleis straight.Dull or bent needles can cause skipped stitches and broken thread.Needle Condition Needle is free of burrs.Needle burrs typically occur when aneedle is deflected and strikes part ofthe machine. These burrs can causethread breakage.Needle Alignment Needle eye is alignedproperly with the hook.Misaligned needles may cause skipped stitches or thread breaks.Thread Tension Settings The thread tension onbobbin and top are assufficient to createbalanced stitches andtight seams.Tensions that are set too high can causethread to break or seams that are tootight. Tensions that are too low cancause loose and uneven stitches.Thread Guides Condition Guides should be cleanand free of burrs.Burrs and dirt on the thread guides cancatch the thread and cause unbalancedstitches or the thread to break.Hook Points Points are sharp andstraight.Hooks wear naturally during use and can cause skipped stitches or thread breaks when dull.Condition of Machine Components (Needle bar bearings, hook race, etc.)Machine components areclean and well lubricated.Worn machine components can causebroken thread, uneven seams, andskipped stitches.Bobbin Hook Position and Timing The hook is positionedclose to the needle,without touching theneedle.The bobbin hook can cause skippedstitches if too far from the needle.W. L. Gore & Associates, Inc. 100 Airport Road, PO Box 1010, Elkton, MD 21921, USA US Toll-Free 800.276.8451 T +1.410.506.8400 E *********************/tenara FOR INDUSTRIAL USE ONLY. Not for use in food, drug, cosmetic or medical device manufacturing, processing, or packaging operations. All technical information and advice given here is based on our previous experience. We give this information to the best of our knowledge, but assume no legal responsibility. The operating data given here has been determined under technically ideal conditions. Any deviations will depend on the conditions of the individual application and whether our sewing and processing instructions have been observed. In order to achieve the best possible results we would ask you to contact our product specialists with the full details of your application. They will be only too pleased to help you. Specifications are subject to change without notice.GORE, TENARA, Together, improving life and designs are trademarks of W. L. Gore & Associates. © 2011–2022 W. L. Gore & Associates, Inc.T E N -D S H -002-E N -J U L 22。
普理灵缝线的使用技巧-回复普理灵缝是一种广泛应用于建筑行业的填缝材料,它具有耐水、抗裂、耐候性强等优点,常被用来填补建筑结构中的缝隙,提高建筑的密封性和美观性。
在日常施工中,正确使用普理灵缝线非常重要,下面将为大家介绍一些使用技巧。
使用普理灵缝线的第一步是准备工作。
首先,要确保准备工具齐全,包括普理灵缝线、剪刀、刮板等。
接下来,清理缝隙,将杂质、尘土等撇除,确保缝隙干净整洁,以便于填充普理灵缝线。
第二步是选择合适的普理灵缝线。
根据不同的施工环境和要求,可选择不同种类、规格的普理灵缝线。
一般来说,常用的有单组分普理灵缝线和双组分普理灵缝线。
单组分普理灵缝线适用于室内环境,而双组分普理灵缝线则适用于室外环境或高温环境。
第三步是将普理灵缝线填充到缝隙中。
在填充之前,要根据缝隙的宽度选择合适的普理灵缝线直径。
通常来说,普理灵缝线直径应比缝隙宽度略大一些,以确保填充充实。
然后将普理灵缝线放入缝隙中,可以使用剪刀剪断并将其塞入缝隙,直到填充充实。
第四步是压实普理灵缝线。
使用刮板等工具将填充好的普理灵缝线稍微压实,确保其与缝隙紧密贴合,减少可能出现的空洞或松动。
注意不要用太大的力气压实,以免损坏普理灵缝线。
第五步是修整普理灵缝线。
在填充和压实完成后,可以使用刮板等工具将多余的普理灵缝线修剪掉,并使其与建筑物的表面平齐。
这样可以提高建筑物的美观性和整体效果。
在使用普理灵缝线的过程中,还需要注意以下几个问题:1. 温度控制:普理灵缝线的具体使用温度范围可通过产品说明书了解,应避免在超过其允许温度范围的环境中使用。
同时,在低温环境中,普理灵缝线可能变硬,可通过加热缝隙或使用专门的低温普理灵缝线来解决。
2. 干燥时间:普理灵缝线填充后需要一定时间干燥才能完全固化。
在施工过程中,要注意避免触摸或移动已经填充好的普理灵缝线,以免影响其干燥过程和施工效果。
3. 施工顺序:普理灵缝线一般在其他建筑工程完成之后进行填充,以免施工过程中的碰撞或压力对其造成损坏。
非吸收性缝合线和非吸收性自封缝合线上针工艺确认方案编号:PLM-VF-PVP-006南京普立蒙医疗科技有限公司一、非吸收性缝合线和非吸收性自封缝合线“切刺设备确认”方案1、概述:本公司生产和研发的产品“非吸收性缝合线和非吸收性自封缝合线”,材料采用聚酰胺,该材料是一种脂肪族聚醚酯,以其优异的生物相容性,以及优异的柔韧性、抗张强度、被成功地应用于临床的手术缝合,并已被国家食品药品监督管理局批准作为医用非吸收性手术缝合线的基本材料,而且批准可用于人体内,并且是理想的手术缝合线材料。
“非吸收性自封缝合线”是使用“聚酰胺”为原料经螺杆纺丝、纺制而成的“非吸收性缝合线”经3D切割而成的自封缝合线与医用缝合针组成,缝合针采用302不锈钢材料制成。
本次验证目的对制成非吸收性缝合线和非吸收性自封缝合线的“上针机”物理性能进行确认和评价,获取上针过程的设备性能保证,最终达到产品符合标准要求。
2、目的:本次验证目的对缝合线上针机进行上针过程确认,对设备性能和上针后的半成品缝合线针线链接的性能进行确认和评价,获取上针过程的设备性能保证,最终达到非吸收性缝合线产品符合产品技术要求的规定。
3. 范围适用于本公司非吸收性缝合线和非吸收性自封缝合线上针工序生产过程,和非吸收性缝合线上朕设备性能确认,确保上针过程的输出能达到预期要求。
4. 过程确认人员资格鉴定记录4.1 确认组长:;4.2 切刺确认组人员:4.3品质经理负责组织确认全过程工作;4.4工程师负责设备和上针工艺技术保证;4.5生产部负责设备保证;4.6采购部负责验证所需物资的供应;4.7品质部负责确认过程的各项检测,负责上针过程的物理性能和生物性能鉴定、切刺前生物负载、环境监测等试验;4.8生产技术部负责组织设备试验和原料准备;4.9生产技术部负责上针设备调试验证工作;4.10确认小组负责人负责协调组织各项验证试验;4.11验证工作小组负责人审阅验证记录,进行分析、评价,负责验证报告的审核;4.12验证领导小组组长负责验证报告的批准。
普理灵缝线的使用技巧普理灵缝线是一种常用的缝线材料,其使用技巧对于缝纫工作非常重要。
下面将介绍几种普理灵缝线的使用技巧,希望能帮助大家更好地运用这种缝线。
首先,选择合适的普理灵缝线是非常关键的。
普理灵缝线的规格有多种,我们应根据所需缝制物品的材质和用途来选择合适的规格。
一般而言,细致的缝线适用于轻薄的面料,而粗细适中的缝线则可以用于厚重的面料。
其次,正确使用普理灵缝线的插线器是非常重要的。
在插线器上必须配备正确的缝线针,以确保缝线能够顺利通过针眼。
在插线器使用时,我们需要仔细观察缝线的通行情况,保持缝线的稳定通过,确保缝线的质量。
接下来,要注意普理灵缝线的拉紧力度。
缝线的拉紧力度应该适中,既不能过紧,也不能过松。
过紧的缝线会导致布料变形,而过松的缝线则会影响缝线的牢固度。
因此,我们需要根据实际情况和缝制要求来掌握好缝线的拉紧力度。
此外,普理灵缝线的尾线处理也需要注意。
为了确保缝线的美观和牢固度,我们可以使用缝面机或手工处理尾线。
处理尾线时,需要将尾线剪短并进行固定,防止其在使用过程中松脱。
最后,定期更换普理灵缝线也是必要的。
长时间使用的缝线会因为摩擦、拉力等原因出现磨损,影响缝线的品质和使用效果。
因此,建议定期更换缝线,以保证缝制工作的质量。
总结起来,普理灵缝线的使用技巧包括选择合适的规格、正确使用插线器、掌握好缝线的拉紧力度、正确处理尾线以及定期更换缝线。
通过掌握这些技巧,我们能够更好地运用普理灵缝线,提高缝制工作的效果和品质。
希望以上内容对大家有所帮助。
妇科相关手术缝线使用指南一、妇科手术缝线的类型。
1. 可吸收缝线。
- 天然材质。
- 肠线:- 特点:肠线是一种从动物的小肠黏膜下层或牛的肌腱中提取制成的可吸收缝线。
它的优点是具有一定的柔韧性,容易操作。
但是其组织反应相对较大,在吸收过程中可能会引起局部的炎症反应。
- 适用手术:常用于一些相对简单的妇科手术,如会阴侧切后的缝合,在一些基层医院可能仍有使用。
- 合成材质。
- 聚乙醇酸(PGA)缝线:- 特点:这种缝线强度较高,在体内吸收相对较快,一般在2 - 3周左右开始失去大部分张力,2 - 3个月内完全吸收。
它的组织反应较小,不易引起感染。
- 适用手术:适用于妇科的多种手术,如子宫切除术、卵巢囊肿剔除术等腹部切口的缝合,尤其是皮下组织的缝合。
- 聚乳酸羟基乙酸(PLGA)缝线:- 特点:具有良好的柔韧性和较高的初始强度,其吸收时间比PGA缝线略长,大约在3 - 4周开始降解,4 - 6个月完全吸收。
在吸收过程中能较好地维持伤口的张力。
- 适用手术:在妇科盆底重建手术中应用较多,如阴道前后壁修补术等,可用于缝合肌肉和筋膜组织。
2. 不可吸收缝线。
- 丝线:- 特点:丝线是一种传统的不可吸收缝线,价格相对便宜。
它的优点是打结牢固,容易操作,具有一定的柔韧性。
但是它会长期留在体内,如果发生感染,可能成为异物,影响伤口愈合。
- 适用手术:在一些妇科手术中,如子宫颈的缝合(如宫颈环扎术),有时会使用丝线,因为它能提供较为持久的张力。
不过目前也有很多医院开始使用可吸收缝线替代丝线进行宫颈环扎术,以避免二次拆线的风险。
- 聚丙烯缝线(普理灵):- 特点:这种缝线强度很高,几乎无组织反应,不易被细菌附着。
它的柔韧性较好,在体内长期保持其物理性能。
- 适用手术:常用于妇科大血管的结扎,如在子宫切除术时结扎子宫动脉等较大血管,也可用于张力较大的切口皮肤缝合,如妇科恶性肿瘤手术后的腹部切口缝合。
二、缝线的选择依据。
1. 手术部位。
可吸收缝合线简介一、缝合线简介医用缝合线是一种用于人体手术缝合的线型材料,根据生物降解性能,可分为非吸收缝合线(金属线、棉线、聚酯、聚丙烯等)和可吸收缝合线(羊肠线、聚乙交酯等);从其物理形态来看,可以分为单股和多股;根据原材料的来源分为天然缝合线(动物肌腱缝线、羊肠线、蚕丝和棉花丝线)和人工合成缝合线(尼龙、聚乙烯、聚丙烯、PGA、不锈钢丝和金属钽丝);根据医生手法,还可分为普通线和倒刺线。
天然可吸收线是由健康哺乳动物的胶原或人工合成的多聚体制备而成,通过人体内酶的消化来降解缝线纤维。
人工合成的可吸收性缝线则先是通过水解作用,使水分逐渐渗透到缝线纤维内而引起多聚体链的分解。
与天然的可吸收性缝线相比,合成的可吸收性缝线植入后的水解作用仅引起较轻的组织反应。
由于天然肠线有抗原性、组织反应较强以及收速率难测等缺点,人们致力于研制人工合成的可吸收性缝线。
主要包括聚乳酸(PLA)缝合线、聚乙醇酸(PGA)缝合线、聚乳酸乙醇酸酯(PLGA)缝合线、聚对二氧环已酮(PPDO)缝合线等,应用X围广泛,从胸腹部伤口缝合以至眼科手术中的应用等。
二、HS产品优势PPDO可吸收缝合线是由聚对二氧环已酮(PPDO)材料纺制而成的一种单股结构可吸收缝合线,具有良好的物理机械强度、化学稳定性、生物相容性和安全性,可生物降解,易于加工成型等优点,是目前唯一可提供最长伤口支持时间的可吸收缝合线,是医用缝合材料领域的新产品。
1. 单丝结构表面光滑圆顺,克服了编织结构缝合线表面磨擦系数大而导致缝合时易损伤组织的缺点;穿透性强,能顺滑穿透组织,使组织准确对合,不造成损伤。
最适宜采用连续缝合技术的手术。
2. 单丝结构在缝线材料上避免了细菌的栖身,消除了因缝线而引起的感染。
3. 具有优良的强度和韧性,抗拉强度大,对伤口的支持力时间长,在组织中保持的强度比其它可吸收缝合线大一倍,手术四周后仍保持原强度的50%以上。
这一特性使它最适用于愈合较慢组织的缝合,如筋膜闭合、骨科、腹部缝合以及糖尿病患者、癌症患者、肥胖患者的手术。
非吸收性外科缝线适用范围:供人体组织的缝合、结扎用。
1.1产品型号、规格及其划分说明1.1.1根据缝合线的粗细分为5/0、3/0、2/0、1、2、3、5、6、7、8十种规格。
1.1.2根据缝合线的长度分为40cm、45cm和75cm三种规格。
1.1.3根据缝合针的针型不同分为圆体角针和角针,如图1、图2。
图1圆体角针图2角针1.1.4非吸收性外科缝线分为带针和不带针,带针的非吸收性外科缝线根据其针线连接型式分为单针和双针,双针连接型式为缝线两端各有一枚缝合针。
1.1.5型号划分说明如下:1.1.6具体规格型号及尺寸见附录A。
1.2结构组成及材料非吸收性外科缝线由缝合线和缝合针组成,其中缝合线由OOCr17Ni14Mo2(316L)单股不锈钢制成,缝合针材料为30Cr13不锈钢,按YY0167-2005中的分类规定属于Ⅲ类单股金属缝线。
2.1缝线2.1.1外观2.1.1.1缝线表面应光滑,条干均匀,无污渍,无结头。
2.1.1.2针线连接处应光滑、无毛刺。
2.1.2 线径缝线的线径应符合YY0167-2005中的规定,见表1。
表1缝线的规格与线径范围2.1.3 抗张强度缝线的抗张强度应符合YY0167-2005中的规定,见表2。
表2缝线的抗张强度2.1.4 长度缝线长度应不小于标识长度的95%,单根缝线的长度应不大于3.5m。
2.2缝合针2.2.1 使用性能2.2.1.1刺穿力缝合针针尖应尖锐、无弯钩,其刺穿力应符合YY0043-2005中要求,见表3。
表3刺穿力2.2.1.2切割力三角针刃口应锋利,其切割力应符合YY0043-2005中的要求,见表4。
表4切割力2.2.2 物理性能应符合YY0043-2005中第4.2条的要求。
2.2.3 外观应符合YY0043-2005中第4.3条(除4.3.4弹机孔嵌线)的要求。
2.3 针线连接强度缝合线的针线连接强度应符合YY0167-2005中4.4条的要求,见表5。
可吸收缝合线说明书1. 产品名称可吸收缝合线,型号:XX-XX。
2. 产品简介可吸收缝合线是一种用于外科手术缝合的医疗器械,采用高分子材料制成,可在体内自然降解,无需拆线,减轻了患者痛苦,提高了手术效果。
本产品经过严格的消毒处理,安全有效,使用方便。
3. 产品特点* 可吸收性:可吸收缝合线在体内可自然降解,无需拆线,减轻了患者痛苦。
* 高强度:高分子材料制成,具有较高的强度和耐磨性,能够满足外科手术的需要。
* 生物相容性:可吸收缝合线与人体组织具有良好的相容性,无刺激性,无致敏性。
* 抗菌性:可吸收缝合线具有抗菌性能,能够有效预防术后感染。
* 使用方便:可吸收缝合线操作简单,易于掌握,节省手术时间。
4. 使用方法* 准备:根据手术需要选择合适规格的可吸收缝合线,检查包装是否完好,如有破损或过期,不得使用。
* 操作:按照外科手术常规方法进行缝合,注意线结的位置和力度,以免造成组织损伤。
* 注意事项:操作过程中需保持清洁卫生,避免污染;同时应遵循无菌操作规范,确保手术安全。
5. 适用人群和适用范围本产品适用于各类外科手术的缝合,如腹部、胸部、神经、血管等部位的手术。
不适用于对可吸收缝合线过敏的人群。
6. 不适用人群和禁用情况* 对可吸收缝合线过敏的人群禁用。
* 有严重心、肝、肾功能不全的患者禁用。
* 孕妇、哺乳期妇女和儿童使用需谨慎。
7. 注意事项* 使用前应检查包装是否完好,如有破损或过期,不得使用。
* 本品为一次性使用产品,不得重复使用。
* 使用过程中需遵循无菌操作规范,确保手术安全。
* 如发现不良反应或过敏反应,应立即停止使用并就医。
8. 保养与维护* 本品为一次性使用产品,用后应妥善处理。
* 建议存放在干燥、通风、无尘的地方,避免阳光直射和高温。
9. 问题与处理如在使用过程中遇到问题,如断线、过敏等,应立即停止使用并联系医生处理。
同时应妥善保存产品包装及说明书以便查阅。
10. 生产厂家和联系方式生产厂家:XXXX医疗用品有限公司地址:XXXXXX电话:XXXXXX邮箱:XXXXXX。
普立蒙缝线说明书
普立蒙缝线是一种用于手术缝合的医疗产品。
以下是普立蒙缝线的说明书:
1. 产品介绍:普立蒙缝线是由医用聚酮酯制成的缝合线,具有高强度和优良的生物相容性。
它适用于皮肤和软组织缝合,用于外科手术和伤口修复。
2. 规格和包装:普立蒙缝线有不同的规格和包装供选择,根据不同手术需求和伤口大小,可有不同的线径和长度选择。
3. 使用方法:在进行手术缝合之前,请确保伤口干净,并遵循无菌操作程序。
将普立蒙缝线穿过针眼,并匹配正确的手术针使用。
将缝线穿过组织,并完成缝合。
缝合时请注意保持线的紧张度,以确保良好的伤口闭合。
4. 注意事项:
- 在使用普立蒙缝线过程中,注意避免线的过度拉伸或扭曲,以免影响缝合效果。
- 请勿重复使用已使用过的缝线,以防止交叉感染和减少止
血效果。
- 针头应根据手术需求选择适当的型号和形状。
- 使用普立蒙缝线时请注意穿刺力度,避免损伤周围组织。
- 根据手术需求,可以选择特殊处理的普立蒙缝线,如覆盖
抗菌物质或具有吸收性的缝线。
5. 存储和保养:普立蒙缝线应储存在干燥、阴凉的地方,避免
阳光直射和高温。
请注意避免受潮和接触化学物质。
在使用前,请检查包装是否完好无损。
过期或包装破损的产品应丢弃,不得使用。
以上是普立蒙缝线的基本说明书,如有更具体的使用指引,请参考产品包装上的相关信息或咨询医疗专业人员。