甘肃某复杂铜铅锌硫化矿石浮选新工艺研究
- 格式:pdf
- 大小:658.41 KB
- 文档页数:6
采矿工程M ining engineering甘肃某含金硫化铜矿石浮选试验研究黄建芬,黄国贤(西北矿冶研究院,甘肃 白银 730900)摘 要:针对甘肃某含金硫化铜矿石黄铁矿、磁黄铁矿等硫铁矿含量较高、难以有效抑制等特点,采用一段磨矿、一次粗选、两次扫选、两次精选流程,药剂制度以石灰和焦亚硫酸钠作硫铁矿抑制剂,丁基黄药为捕收剂,J31为捕收起泡剂,在较低pH值条件下实现了对矿石中铜、金的高效回收。
闭路试验获得铜精矿铜品位22.18%,铜回收率92.57%;金品位7.75g/t,金回收率80.41%。
关键词:某含金硫化铜矿石;硫铁矿抑制剂;J31捕收起泡剂;铜回收率;金回收率中图分类号:TD923;TD952 文献标识码:A 文章编号:1002-5065(2020)20-0052-3Experimental Study on Flotation of a Gold Bearing Copper Sulfide OreHUANG Jian-Fen, HUANG Guo-Xian(Northwest Research Institute of Mining and Metallurgy, Baiyin 730900,China)Abstract: In view of the high content of pyrite and pyrrhotite in a gold bearing copper sulfide ore in Gansu Province,the flowsheet of of one stage grinding,one roughing,two sweeping and two concentrating were adopted.The reagent system was:Lime and sodium pyrosulfite are used as pyrite inhibitors,butyl xanthate as collector and J31 as acapturingand foaming agents.Under the condition of low pH value, copper and gold in the ore can be recovered efficiently. The copper concentrate contains 18.13% copper and 4.87 g/t gold, and the recovery rates of copper and gold are 69.88% and 52.17% respectively.Keywords: a gold bearing copper sulfide ore;pyrite inhibitors;J31 acapturingand foaming agents;copper recovery;gold recovery甘肃某含金硫化铜矿石,黄铁矿、磁黄铁矿含量较高,采用常规的高碱工艺进行浮选难以有效抑制,铜、金矿物与硫铁矿分选效果不佳,尤其是金的回收率较低。
采矿工程M ining engineering 某铜锌矿浮选分离试验研究师伟红,刘守信(西北矿冶研究院,甘肃 白银 730900)摘 要:根据甘肃某难选铜锌矿矿石性质特点,确定了优先浮铜再选锌的原则工艺流程。
铜浮选作业,采用高效的锌矿物抑制剂T20及对铜矿物选择捕收性能较好的高效捕收剂A11,实现了铜锌的有效分离,获得了较好的选矿技术指标,为该类型铜锌矿石资源的开发利用提供了技术依据。
试验最终获得闭路指标为:铜精矿含铜18.04%,铜回收率88.42%,含锌4.95%;锌精矿含锌40.28%,锌回收率69.88%。
关键词:优先浮选;铜锌分离;组合抑制剂T20;高效捕收剂A11中图分类号:TD952 文献标识码:A 文章编号:1002-5065(2019)11-0031-2Experimental Study on Flotation Separation of Copper-Zinc OreSHI Wei-hong, LIU Shou-xin(Northwest Research institute of mining and metallurgy, Baiyin 730900, China)Abstract: According to the ore properties of a copper-zinc mine in Gansu Province, the principle technological process of preferential flotation of copper and zinc is determined. In copper flotation operation, better beneficiation technical indicators were obtained with high-efficiency zinc mineral inhibitor T20 and high-efficiency collector A11, which provided technical basis for the development and utilization of this type of copper and zinc ore resources. The final closed-circuit indicators were: the copper concentrate contains 18.04% copper and 4.95% zinc, and the recovery rate of copper is 88.42%; the zinc concentrate contains 40.28% zinc,and the recovery rate of zinc is 69.88%.Keywords: Preferential flotation; Separation of copper and zinc; Combined inhibitor T20; High-efficiency collector A11铜锌硫化矿石是提取金属铜、锌的重要原料,因此其选别分离研究工作十分重要。
铅锌浮选工艺研究报告一、引言铅锌矿是一种重要的金属矿石,在工业生产中具有广泛的应用价值。
铅锌浮选是一种常用的选矿工艺,通过浮选过程可以有效地将铅锌矿石中的有用矿物与非有用矿物分离开来,提高铅锌矿石的品位和回收率。
本报告旨在研究铅锌浮选工艺,探索工艺参数对选矿效果的影响,以及提出优化建议。
二、浮选原理铅锌浮选工艺基于矿石中铅锌矿物与非有用矿物的物理和化学性质差异,利用浮选剂和气泡在水溶液中的相互作用实现矿物的分离。
一般情况下,通过调整浮选剂的种类和添加量,可以使铅矿和锌矿在浮选过程中完全浮起,而非有用矿物则沉于底部或被抑制。
三、工艺参数1. 浮选剂种类:浮选剂的选择是影响浮选效果的重要参数。
常用的浮选剂包括黄药油、木油、石油磺酸盐等,不同的浮选剂对不同矿物的选择性有所差异,应根据具体矿石性质选择合适的浮选剂。
2. 浮选剂添加量:浮选剂的添加量会直接影响铅锌矿浮选的效果。
添加过少会导致浮选矿物的回收率降低,而添加过多则可能造成矿石中铅锌矿物与非有用矿物的过度悬浮,降低分离效果。
因此,在实际生产中应通过试验确定合理的浮选剂添加量。
3. 搅拌强度:搅拌强度是指在浮选槽中传递气泡与矿物以及浮选剂之间的力。
适当的搅拌强度有助于气泡与矿物的接触,提高浮选效果;过强或过弱的搅拌强度都会影响浮选效果,应根据矿石特性确定合适的搅拌强度。
4. 气泡尺寸:气泡尺寸是影响铅锌浮选的关键参数之一。
较小的气泡有更大的表面积与矿物接触,提高选矿效果,而较大的气泡则容易被矿物顶起,导致浮选效果下降。
因此,在浮选过程中要控制气泡的大小,获得最佳的浮选效果。
四、工艺优化建议1. 优化浮选剂种类和添加量:根据不同矿石性质,选择具有较好选择性的浮选剂,并通过试验确定合适的添加量,以提高浮选效果。
2. 控制搅拌强度:根据矿石特性,确定适宜的搅拌强度,保证气泡与矿物的充分接触,提高浮选效果。
3. 精确控制气泡尺寸:通过优化气泡生成设备或微调工艺参数,探索合适的气泡尺寸范围,以获得较好的选矿效果。