摘要:结合新建玉林至铁山港铁路工程,采用贯入法对隧道初期支护喷射混凝土早期(1d)强度进行检测方法的研究。HQG-1000型混凝土强度检测仪采用压缩弹簧加载,把钢制测钉贯入混凝土中。因贯入深度与混凝土强度相关,即可根据测钉贯入深度来推定混凝土强度。大大缓解了工地隧道试验员的工作强度,更及时有效的指导了施工生产。

关键词:贯入法喷射混凝土早期强度检测

Abstract: Combining the Yulin to TieShanGang new railway engineering, the penetration method of the tunnel of the concrete and the primary support early (1 d) strength the study of the method of detection. HQG-1000 type concrete intensity detector using compression spring loading, the steel nails penetration concrete. For penetration depth and strength of concrete related can according to the nail penetration depth to presumed the strength of concrete. Greatly alleviate the tunnel of the operator site working strength, the more timely and effective guidance to the construction production.

Key Words: penetration method, sprayed concrete, early strength, testing

引言

《铁路隧道工程施工质量验收标准》规定,“喷射混凝土的早期(1d)强度必须符合设计要求”,“采用贯入法或拔出法检测”。铁建设[2010]257号文发布的铁道部《关于发布铁路桥涵设计基本规范等11项铁路工程建设标准局部修订条文的通知》中规定,“隧道支护喷射混凝土的强度等级不应低于C25,24小时强度不小于10MPa”。

喷射混凝土初期支护是保证围岩稳定,保证施工安全的重要措施之一。

为了加强隧道初期支护喷射混凝土1d强度控制、落实验标要求,试验室开展了“贯入法检测隧道喷射混凝土早期强度”的研究。

国内检测技术现状

拔出法检测,铁道部已有《混凝土强度后装拔出法试验方法》TB/T2298.2~1991。经应用,由于隧道初支喷射混凝土表面不平整、粗糙,早期强度低等特点,现场表面打磨困难、钻孔及孔内切槽难以达到测试条件,拉拔杆安装与基座难以垂直,造成测试数据过于偏离实际。拔出法操作较复杂,部件多,须多人操作。实践证明拔出法不适用于隧道喷射混凝土早期测强。

建设部有《贯入法检测砌筑砂浆抗压强度技术规程》JGJ/T136-2001。由于测针小,冲击功能低,不能满足喷射混凝土早期测强要求。